BINDER MIXTURE WITH PHOSPHOGYPSUM


Purpose of the development: Astringent gypsum mixture used to make various decorative (panels, moldings and etc.) And carriers (plates, blocks, etc.). Gypsum products.

Recommended application field: Binder mixture of gypsum is widely used in building and construction materials

Technical characteristic: Specifications: Composition plaster finely dispersed polymer mixed with white color or odor presence Humidity 2-3% Water plaster ratio (vodopotreby) 0,75-0,85 l / kg term seizure top 3-8 min .; end of 15-20 minutes. Fineness of grinding residue on sieve 0.08 to 2% (ind.III, fine grinding) bending strength (age 2 hours) 2.3 - 3.5 MPa

Advantages over analogues: Fundamentals them the benefits of a "yazhuchi plaster over similar products are: - ability to control the setting time - high strength products - cheap raw materials from the use of dump waste and lack of stage grinding - reduce water consumption by 60-70% compared with traditional methods phosphogypsum purification from impurities.

The development stage readiness: Tested experimental exploitation order

Description of the development:
()
Method of processing phospho gypsum binder in plaster mixture is purified it from contaminants in the environment of an aqueous solution, activated sludge and polymer impurities introduced to improve specifications.

corresponds technical description
Conforms to technical characteristic

Possibility of transfer abroad:
Licence's sale
Technological document's sale
Combinated reduction to industrial level

Photo

Country Ukraine

For additional information turn to:
E-mail: gal@uintei.kiev.ua

or fill out the form:
Organization name :
Address :
Settlement account :
Bank :
MFO :
OKPO code :

Scientific organization tutor's data :
Surname :
Name :
Patronymic :
Scientific degree :
Phone :
Fax :
E-mail :
Cooperation proposals (joint patent, joint enterprise, assembly sale and so on :
country: