DEVICE FOR OBTAINING OF THE THERMALLY EXPANDED GRAPHITE
Purpose of the development:
Creating a device for producing expanded graphite with a reduced degree of contamination of the products of sulfur without any heat loss.
Recommended application field:
Protective coating surfaces.
Technical characteristic:
The total gas costs for obtaining 1 kg of graphite - 7 m3 per hour.
Carbon content,% al - 99,5-99,7.
Sulphur content,% al - <0.1-0.2.
Metal content,% at - -.
Bulk density p, g / cm3 - (3-5) 10 -3 degrees.
The density of the pressed samples, g / cm3 - 0.3-2.0.
Advantages over analogues:
Complete removal of a chemically bonded and adsorbed sulfur products.
Energy-saving technology with the ability to create in Ukraine a fully closed cycle.
The development stage readiness:
Tested experimental exploitation order
Description of the development:
() Proposed cyclone furnace for graphite teromorozshirennogo whose advantage is that graphite, that is processed, stored in the high temperature zone (C * 10000) is much longer (8-10 seconds) as compared with known fluidized bed furnaces (1.2-2 seconds ).
corresponds technical description
Conforms to technical characteristic
Photo
Country
Ukraine
For additional information turn to: E-mail: gal@uintei.kiev.ua
|